When skin is cut, the body builds a scab. The scab protects the wound, and once it is thick enough, the repair slows down. Now imagine the scab is knocked off again and again. Each time the body must rebuild it, and each rebuild costs resources. The graphite anode of a lithium-ion cell lives with a similar problem. It is covered by a solid-electrolyte interphase (SEI), a thin film that protects it but is built from lithium. A recent vibration study uses an SEI growth model to show how shaking keeps reopening that wound and drains the cell.
What the SEI is and why it matters
The SEI forms when electrolyte decomposes on the anode surface. In a healthy cell, it grows quickly at first, then slows as the film thickens and becomes harder for solvent to cross. This self-limiting behaviour is what makes a normal cell last.
The catch is that every bit of SEI is built from lithium that can no longer shuttle between electrodes. That loss is called loss of lithium inventory, and it is one of the main routes to capacity fade.
Growth on the original surface and on cracks
The model follows SEI thickness on two kinds of surface: the original particle surface and new surfaces exposed by cracks. For the crack surfaces, thickness changes through two contributions:
- Diffusion-limited growth. Solvent must travel through the existing film to react. The rate falls as the film gets thicker, so thick layers grow slowly and thin layers grow fast.
- Crack-driven renewal. As cracks lengthen, new surface appears with only a thin initial film. This pulls the average back toward the thin starting value and restarts rapid growth on the fresh area.
Together these describe a cycle: crack, expose, rebuild, thicken, and then crack again.
From side reaction to thickness
The wider model converts the electrochemical side reaction into a physical film in a few steps:
- A side-reaction current at the anode depends exponentially on the SEI overpotential and temperature, so warmer cells form SEI faster.
- Faraday’s law converts that current into moles of SEI species.
- Using the molar mass, density and internal surface area, the amount of SEI becomes a film thickness.
- Ohm’s law then gives the film’s resistance, which grows with thickness and falls with conductivity and active area.
The chain ends in two penalties: lithium is consumed, and impedance rises.
What the loss looks like
The study links capacity loss directly to SEI growth through a simple relation, where the rate of capacity decline is proportional to the rate of thickness increase. Faster film growth therefore means faster capacity fade.
A quick illustration, using my own numbers rather than the paper’s: if growth through the film follows the inverse of thickness, an established 100 nm layer grows about ten times slower than a fresh 10 nm one. This is why a cell without vibration settles down while a repeatedly cracked one keeps spending lithium on new films.
Heat and resistance come along
A thicker SEI increases cell resistance, and the study adds that this raises ohmic heating. The authors argue that the temperature rise seen at later cycles is driven mainly by this growing resistance, not by friction alone. Warmer cells then speed up the side reaction, which closes a feedback loop between mechanics, chemistry and heat.
What the simulations report
In the paper’s results, SEI thickness grows faster under vibration than without it, and growth speeds up with both amplitude and frequency. The authors also describe SEI-driven lithium loss as the dominant degradation pathway under the conditions studied. Related experiments in the literature have reported SEI thinning in some chemistries and regimes, and the authors argue that the present conditions are dominated by cumulative growth instead.
Reading it with care
- The thickness is an average. The model reports a spatially averaged value, while real films vary with local current and stress.
- Other mechanisms are set aside. Lithium plating and dead lithium are not modelled, and the authors list them as future work.
- Parameters are partly assumed. Dedicated vibration measurements of SEI are limited, so results should be treated as trends.
Takeaway for design
If every crack restarts the SEI cycle, the best protection is to prevent cracks. Tougher particles, binders that share load, electrolytes that form stable films and mounts that damp vibration all reduce how often the film is broken. For anyone interpreting field data, rising resistance with falling capacity under vibration may be the visible sign of a scab that cannot heal.